A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: RIE Question
Probe Arms with Kinematic bearings? Where to buy it?
2007-08-30
Guangchi Archie Xuan
RIE Question
2007-08-30
Joseph Grogan
2007-08-30
Michael D Martin
2007-08-31
PRAMOD GUPTA
2007-09-04
Bill Moffat
2007-08-30
[email protected]
2007-09-02
Nicolas Duarte
RIE Question
PRAMOD GUPTA
2007-08-31
I am also looking for a recipe to etch 10um deep polymer with vertical wall
profile(linewidth~8um with Al or NiCr mask, spacing~250um) with SF6/O2/CHF3 gas
chemistry using "Oxford Plasmalab 80 plus" system. If any one has any kind of
recipe or research paper please let me know.

Michael D Martin  wrote:  I would increase flow
rates to reach a pressure of 100-200mT and boost power to 250-350W. The white
powder is likely sputtered silicon /silicon dioxide redeposition. You might
consider running a cleaning cycle before processing. It's been our experience
that this improves repeatability, particularly for a multiuser piece of
equipment.


Pramod Gupta
21084 Red Fir Court
Cupertino, CA 95014
Phone: (408) 253-1646

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
MEMS Technology Review
MEMStaff Inc.