MEMSnet Home: MEMS-Talk: EDP etch compatibility
EDP etch compatibility
2007-09-12
Ho Yin Chan
2007-09-12
Michael D Martin
2007-09-12
Nicolas Duarte
EDP etch compatibility
Nicolas Duarte
2007-09-12
I know that gold is etched by EDP however I have had no personal
experience with Ti or Ag.

-Nicolas "Nik" Duarte
Ph.D. Candidate at Penn State University
Department of Electrical Engineering

On Sep 11, 2007, at 11:35 PM, "Ho Yin Chan"  wrote:

> Hi,
>
> Currently, I am doing EDP process with Ti/Au/Ag stacks on SiO2. It
> is found
> that the metal stack pattern has gone after EDP etch.  Could you
> share with
> me your experience? I am guessing if the problem is caused by Ti.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
The Branford Group
Addison Engineering
Harrick Plasma, Inc.