Dear All,

I want to plate very small cavities (200nm diameter and 500nm deep) with a
conductive material.
Can this been done by electro- or Eless plating?
Or must we use a sputter or evaporation process?

Thanks in advance.

Peter Kuijpers
MiPlaza
DTS/TFF
High Tech Campus 04
Room: WAGp5-11
5656 AE Eindhoven
The Netherlands

Phone.:  (+31 40 27) 98904 (mobex)
mobile:(+31) 06-12507027
fax.:     [+31 40 27) 44769
mailto:[email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation