Hi Yuming,

In order to avoid photoresist interaction with OTS solution solvent
(chloroform) I would suggest to deposit hydrophobic layer in a vapor phase
(for example, MVD-100 vapor deposition system will do a good job for you).
Alternative method to pattern Self-assembled monolayers (without photoresist
processing) is UV Ozone stripping through a mask.

Boris Kobrin, Ph.D.
Sr.Dir Marketing & Bus.Dev.
Applied Microstructures, Inc.
1020 Rincon Circle, San Jose, CA 95131
Office: (408) 907-2885 x2805
Mobile: (408) 806-6859
[email protected]

Message: 5
Date: Wed, 19 Sep 2007 21:20:36 +0800
From: "Steven Yang" 
Subject: [mems-talk] Safe OTS solution for hydrophobic pattern with PR?

Hi,all
I am facing problem to pattern OTS hydrophobic region in a
microchannel. The method I plan to use is PR (AZ 5214 or AZ 7220)
pattern a open window on part of microchannel (100um width of channel,
OTS pattern 100x100um or 100x200um). and the OTS solution will be OTS
2mM in Hexadecane:Chloroform (4:1 by Vol). However, the problem is
that I was told that chloroform might strip the photoresist during dip
in OTS coating. Does anybody have this experience or the alternative
OTS solution recipe to avoid photoresist stripping?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Mentor Graphics Corporation
The Branford Group