Splash back problems with resist spin
2007-09-19
Edward Sebesta
2007-09-20
dbplists
SV: [mems-talk] Splash back problems with resist spin
2007-09-20
eowin rohan
2007-09-20
Brent Garber
2007-09-20
Seth Burtner
2007-09-20
dbp lists
Splash back problems with resist spin
Brent Garber
2007-09-20
Ed,

Slow down and lets fix your problem with the spinner you have.  What is
the size of your wafer and what size is your chuck?

Brent

Edward Sebesta wrote:
> I have an MTS 8800 with splashback problems, that is photo resist
> redopositing on to the back side of the wafers.
>
> I have check the exhaust and made sure it was the maximum. I have tried
> recipe modifications with lower acceleration for the resist spin step.
> These are the standard causes for the problem.
>
> I would like to know the following.
>
> 1. Does anyone have a contact for persons manufacturing retrofit resist
> spin bowls?
>
> 2. Does anyone have a fix for this or suggestions.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Addison Engineering
Tanner EDA by Mentor Graphics