SU-8 on glass
2007-10-08
Yue Mun Pun, Jeffrey
2007-10-08
Silvan Schmid
2007-10-09
Satyanarayan Nagarajan
2007-10-09
GARCIA BLANCO Sonia
2007-10-08
Jian Wang
2007-10-15
Gareth Jenkins
2007-10-15
Jianhua Tong
2007-10-16
Yue Mun Pun, Jeffrey
SU-8 on glass
Yue Mun Pun, Jeffrey
2007-10-08
Hi,
I am using SU-8 2000 series and may need to use it on glass wafers.  Can anyone
suggest how I can make SU-8 adhere to glass, whether I need to spin coat
Omnicoat or treat the glass with oxygen plasma?
Also, how do I dice the glass wafers?  I have tried using a manual diamond
scriber but it does not cut the glass in straight lines.

Mr. Jeffrey Mun Pun YUE
余文彬
Division of Bioengineering
E3A-07-02, Nanobioanalytics Lab
7 Engineering Drive 1
National University of Singapore
Singapore 117574
Tel: (65) 65166482, Fax: (65) 68723069
E-mail:  [email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
The Branford Group
Nano-Master, Inc.