MEMSnet Home: MEMS-Talk: cantilever electrodes
cantilever electrodes
2007-10-18
vaibhav mathur
cantilever electrodes
vaibhav mathur
2007-10-18
I want to utilize MEMS  AlGaAs micro cantilevers that I fabricate on GaAs , as
electrodes. For this, I believe I have to dope the AlGaAs layers very highly n
type or p type, to achieve high conductivity. I want to bias the electrodes and
generate a strong electric field in the vicinity of the device.. Can someone
help in deciding the doping concentration for this.

Also, how closely in strenght and field generated do highly doped semiconductors
behave when compared to traditional electrodes made out of copper or gold??


Regards
Vaibhav Mathur

_________________________________________________________________
Windows Live Spaces is here! It’s easy to create your own personal Web
site.
http://spaces.live.com/?mkt=en-in
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
Process Variations in Microsystems Manufacturing
MEMS Technology Review