Low Etch Rate but High Interface Trap Density for PECVD oxide film?
2007-10-27
Chih-Chieh Cheng
Low Etch Rate but High Interface Trap Density for PECVD oxide film?
Chih-Chieh Cheng
2007-10-27
Hi,

We have very quality of good PECVD oxide films (etch rate for HF:DI
water:1:20: 230 A/min) but the trap density is quite poor. We do not
have the quantitative data for the trap density but based on what we
observed from our fabricated MEMS switches. Could anyone please
comment on it?

Thanks

CC
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
The Branford Group
University Wafer