Hi:

I recently tried to use nickel plating solution from transcene to
plate poly-Si.  Afterwards I tried etching the nickel off with piranha
etch but it left a hazzy film on the poly-Si, which I suspect is
nickel oxide.  Is there any way to etch off the nickel oxide without
etching the poly-Si?

Thanks and regards,
Johnson Wong
PhD Research
School of Photovoltaic Engineering
University of New South Wales
NSW 2052, Australia
Office (04) 9385 7942
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Mentor Graphics Corporation
Addison Engineering