Ning Wu,  You might try high pressure steam oxidation, you could achieve
several bar at reasonable temperatures.  Steam is a very aggressive oxidant,
and something as simple as a pressure cooker might do your job.  Easy and
cheap to try.  Gary

Gary Hillman
Service Support Specialties, Inc.
PO Box 365
9 Mars Court
Montville, NJ 07045
Telephone 973-263-0640 extension 35
Fax 973-263-8888

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics