proper glass-glass bonding
Bob Henderson
2007-11-02
Mikael:

Maybe groups that provide the superior bonding like to be paid for their IP
investment. I alway maintain that deluxe cost 5 cents extra. Bob Henderson
----- Original Message -----
From: "Mikael Evander" 
To: 
Sent: Friday, November 02, 2007 7:58 AM
Subject: [mems-talk] proper glass-glass bonding


> Hello.
>
> I'm familiar with the "standard" glass-glass thermal fusion bonding method
where you wash your glass wafers, preferable surface activate them with
O2-plasma or such-like and thermo-cycle them in an oven a bit over Tg with
some pressure on the wafers. As far as I know most people using this get a
pretty low bonding efficiency, some voids and usually not the nice
"mirror-finish" on the glass that you usually see before you bond.
>
> I'm also aware that the companies doing glass-structuring and bonding
commercially must have, and have, much better bonding efficiencies and
incredably good looking bonding.
>
> I find it kind of surprising that whatever tips and tricks are being used
in getting at least a slightly better bond hasn't seeped out from the
industry. As far as I know at least ...
>
> Does anyone have any nice tips and tricks to share that would help me, and
hopefully lot of other people, to get more efficient bonding?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
MEMStaff Inc.
Process Variations in Microsystems Manufacturing