N K Choudhary (97307404)
Handling & Safety Instructions for EDP etching of Si
N K Choudhary (97307404)
1998-08-06
Hello,
        We need to etch( anisotropic ) Si using Ethylene Diamine + Pyrocathechol
We have procured the chemicals in sealed bottles WITHOUT the saftey /
handling instructions. I would appreciate if somebody could help us
either by giving a reference or the instructions themselves.
        The crunch is heating the mixture to 80 deg C using a reflux system.

Regards
NK Choudhary


******************************************************************************
Electrical Engg.                              Flat No 7,Leo House,
Microelectronics.                             Nana Palsekar Road,
IIT Powai.                                    Opposite IIT Main Gate,
Bombay- 400 076.                              Bombay- 400 076.
email:                 Tel : (022) 577 2339
******************************************************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review
Harrick Plasma, Inc.