MEMSnet Home: MEMS-Talk: black wax for koh etch
black wax for koh etch
2007-11-05
Chin-Jen Chiang
2007-11-07
shay kaplan
2007-11-06
CANAVESE GIANCARLO
2007-11-07
Chin-Jen Chiang
black wax for koh etch
Chin-Jen Chiang
2007-11-07
Dear Giancarlo,

  Thanks a lot for your response.
  Can you please give me some more details about protek? How dose it work (like
wax?) and where I can get it?

  Do you think wax is unable to resist KOH for long KOH etching? I need to have
a long KOH etch for a 500 um Si bulk to remain a 10 um thinkness silicon
membrance with 1mm by 1mm square.

  Best regards
  Lawrence

CANAVESE GIANCARLO  說:
  Dear Chin-Jen Chiang
I think that protek is better than black wax for koh wet
etching protection.

Giancarlo Canavese

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Harrick Plasma, Inc.
Addison Engineering