Difficulties with finding the alignment markings during the photolithography on ceramic substrates
2007-11-12
Denis Petrov
Difficulties with finding the alignment markings duringthe photolithography on ceramic substrates
2007-11-12
Bob Henderson
Difficulties with finding the alignment markings during the photolithography on ceramic substrates
Denis Petrov
2007-11-12
Hello,

I have several ceramic wafers to be exposed. While trying to complete
the subsequent photolithography steps, I have encountered the
following problem.
Due to the roughtness of the ceramic surface, it is very difficult to
recognize the alignment marks (or even the structure patterns) in the
microscope... As a consequence, misalignments occure, and that spoils
all the previous work.
Does someone know how to overcome this, or how to enchance the
visibility of the markings?

Thank you!

Regards,


--
Denis Petrov
Ph.D. Student

Institute for Microsensors, -actuators and –systems (IMSAS)

University of Bremen

http://www.imsas.uni-bremen.de
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
The Branford Group