Au-Au thermocompression bonding
2007-12-12
Joseph Grogan
2007-12-12
Felix Lu
Au-Au thermocompression bonding
Felix Lu
2007-12-12
Hi Joe,

   I've done it on a flip-chip bonder a few times with small pieces. I
don't know what sort of mechanical strength it has but for holding small
MEMS devices, it seems to be satisfactory. I used an Ar RIE plasma to
activate the Au surfaces (150W, ~20 mTorr Ar, 1 minute) then used a
thermocompression bonding sequence in the flip chip bonder to align, and
stuck the pieces together using 3 kg pressure, at 300C for 5-10 minutes.

Felix

Joseph Grogan wrote:
> Is there anybody out there with personal experience performing wafer
> bonding by gold-to-gold thermocompression bonding? I've found several
> papers, and performed several experiments, but I'm getting mixed
> results and I'd like to discuss my process with someone who's done it.
>
> thank you,
> Joe Grogan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Harrick Plasma, Inc.
Nano-Master, Inc.