MEMSnet Home: MEMS-Talk: Re: Mechanical properties of silicon
Re: Mechanical properties of silicon
1998-08-05
John Neumann
1998-08-05
Kirthi Roberts
1998-08-05
John Karpinsky
1998-08-06
Eric Bonnotte
1998-08-06
Wen H. Ko
1998-08-05
Kirthi Roberts
1998-08-05
M.C. Federico Sandoval
1998-08-06
Brian S Cheung
1998-08-17
Ram N. Ramanan
Re: Mechanical properties of silicon
Ram N. Ramanan
1998-08-17
Hi,
Would you be kind enough to summarize all the responses
and post it ? I have been looking for reliable thermal
properties (to be specific, emissivity data)
for Silicon & Si films for quite some time.
Thanks,
Ram
--
-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=
  Ram N. Ramanan, Ph.D.               FSI International
  Microlithography,  R&D              MS 5-7060, 600 Millennium Dr.
  Ph: 972-643-2213                    Allen, TX-75013
  Email: [email protected]        www: http://www.fsi-intl.com
-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing