MEMSnet Home: MEMS-Talk: Lift off process with S-1818
Lift off process with S-1818
2007-12-22
Le Cao Hoai Nam
2008-01-02
Edward Sebesta
2008-01-02
Jianhua Tong
2008-01-03
Le Cao Hoai Nam
2008-01-03
Edward Sebesta
2008-01-03
Wilson, Thomas
Lift off process with S-1818
Le Cao Hoai Nam
2007-12-22
Dear MEMS reseachers,

I am using S-1818 photoresist for a lift off process of Au/Cr on
borosilicate glass substrate. The thickness of S-1818 is around 2um. And the
thickness of Au and Cr is 50nm and 80 nm respectively. After a Cr/Au
evaporation, I soaked the chip in an acetone container in an ultrasonic
bath. I noticed that even after 50min of ultrasonication the photoresist
still remained (the manufacturer recommends 10min of ultrasonication) around
50% on the chip. On the other hand, it seems that I didn't have the undercut
pattern after development. I don't know if this have anything to do with the
remaining of photoresist. I would appreciate it very much if someone could
shed light on this problem. Thank you very much in advance.

Best regards,
Nam Cao Hoai Le, graduate student
Ritsumeikan University, Japan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Mentor Graphics Corporation
The Branford Group