MEMSnet Home: MEMS-Talk: RIE removal of S1818 photoresist
RIE removal of S1818 photoresist
2008-01-16
Curtis, Mark E.
2008-01-16
Bob Henderson
Fluorine residues etching Cr and Au
2008-01-17
Jason Milne
2008-01-17
Bob Henderson
2008-01-18
Martin Lapisa
2008-01-17
Jaibir sharma
RIE removal of S1818 photoresist
Martin Lapisa
2008-01-18
Hello Mark,

Chromium forms a volatile oxide at higher temperatures (>=~190°C). Therefore
you should keep the wafer temperature low by either cooling from the
backside, or running a pulsed plasma, or ashing in several shorter runs,
or....
Unfortunately I do not know your etch equipment but if it is not really
necessary to have 25W on the platen I would decrease it to a minimum. My
wild guess would be that not only the temperature impact would be much lower
without it and also the physical. Maybe you should increase O2 flow and
higher coil power a little instead.

Best regards,
Martin Lapisa

Microsystem Technology Laboratory
School of Electrical Engineering
Royal Institute of Technology (KTH Stockholm)

-----Original Message-----
From: Curtis, Mark E. [mailto:[email protected]]
Sent: Mittwoch, 16. Januar 2008 16:45
To: [email protected]
Subject: [mems-talk] RIE removal of S1818 photoresist

Hello all,

I’m using Shipley S1818 positive photoresist as a mask for wet-etching a 100
nm thick film of chromium.  After using a wet chemical photoresist stripper
there remains some photoresist residue on the surface of the chromium.  I’ve
attempt to use a Trion RIE to remove the photoresist residue with the
following etch parameters:
Gases/Flow Rate (O2/50 sccm),
Pressure (500 mTorr),
RIE Power (25 W), ICP Power (500 W), and Time (30 min).

To my surprise, I found that not only did it remove the photoresist but also
the chromium.  Does anyone know of a good photoresist removal recipe for RIE
that will not etch chromium.  I have previously tried a shorter etch time
(~10 min) but it did not completely remove the photoresist residue.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
MEMS Technology Review
Mentor Graphics Corporation