MEMSnet Home: MEMS-Talk: High Thickness of Aluminum on Silicon
High Thickness of Aluminum on Silicon
2008-01-21
Jacques FATTACCIOLI
2008-01-21
Andrea Mazzolari
2008-01-21
Hong Chen
2008-01-22
Jacques FATTACCIOLI
2008-01-22
shay kaplan
2008-01-22
Gary Hillman
Selective, clean PDMS etch
2008-01-23
Rick Giuly
2008-01-22
David Nemeth
2008-01-21
shay kaplan
High Thickness of Aluminum on Silicon
David Nemeth
2008-01-22
Electroplating is a good solution, but care must be taken with very thick
layers to avoid excessive stress at these thicknesses.

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Hong Chen
Sent: Monday, January 21, 2008 2:23 PM
To: [email protected]; 'General MEMS discussion'
Subject: RE: [mems-talk] High Thickness of Aluminum on Silicon

Electroplating

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Andrea Mazzolari
Sent: Monday, January 21, 2008 11:50 AM
To: General MEMS discussion
Subject: Re: [mems-talk] High Thickness of Aluminum on Silicon

Yes, this is possible with screen printing. Maybe there are other methods,
i don't know.
At physics department of Ferrara University we have the possibility to
realize such depositions.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMStaff Inc.