Javier Sesé
2008-01-24
  We are fabricating a microcoil using two metal layers and PECVD oxide
for electrical insulation. The metal layers are gold deposited using
e-beam evaporation with a few nm of Cromium for adhesion. We found that
the PECVD oxide that grows on top of gold is VERY ROUGH (tipically a
roughness of 50nm for a 200nm thick layer). Further it is plenty of
pinholes. Does anyone know the reason?

We use N2O and 5%SiH4 95%He as precursor gases, deposition temperature
is T=300ºC



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Harrick Plasma, Inc.
MEMStaff Inc.