MEMSnet Home: MEMS-Talk: how to get rid of photoresist residure
how to get rid of photoresist residure
2008-01-24
Chin-Jen Chiang
2008-01-24
Bob Henderson
2008-01-24
Bill Moffat
2008-01-24
Chin-Jen Chiang
2008-01-26
Tolga YELBOGA
how to get rid of photoresist residure
Chin-Jen Chiang
2008-01-24
Hi Bill,

  Thanks for your response.

  My device has very sharp Si field emitter tips with ~150A radius. Using RIE
descum with O2 gas might damage the Si tips due to ion or radical bombardment.
Do you have any comment about this?
  Thanks.

  Lawrence


Bill Moffat  »¡¡G
  What is your device concern? Modern plasma cleaners have electron free
plasma that can safely and gently etch organics with no ESD and minimal
change if temperature.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
The Branford Group
MEMS Technology Review