For gold, just look it up in Physics of Semiconductor Devices by S. M. Sze.

Manu

-----Original Message-----
From: [email protected] [mailto:[email protected]] On
Behalf Of Bahram Ganjipour
Sent: Wednesday, January 30, 2008 3:12 AM
To: [email protected]
Subject: [mems-talk] diffusion constants in GaAs

Hello Everyone,

I am looking for the diffusion constants of gold in GaAs , Platinum in GaAs and
Nickel in GaAs. I would greatly appreciate any guidance
towards papers or reference volumes that might include this information.

I have come up dry with a number of different references, including the
CRC Handbooks.

Thank you very much for your help
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Addison Engineering
Tanner EDA by Mentor Graphics
MEMS Technology Review