MEMSnet Home: MEMS-Talk: Si/Ge pieces surface cleaning
Si/Ge pieces surface cleaning
2008-02-05
Xiaochen Sun
2008-02-05
Edward Sebesta
2008-02-05
Xiaochen Sun
2008-02-05
Bill Moffat
2008-02-07
mosha aharon
Si/Ge pieces surface cleaning
Xiaochen Sun
2008-02-05
Hi Ed,

Thank you very much for your advice. IPA is isopropyl alcohol right? I don't
think we have IPA dryer machine available now. I'll try rinse water off with
IPA and then blow dry with N2 first and see.