MEMSnet Home: MEMS-Talk: Is it possible to deposit Pt directly on Si/SiO2(PECVD) substrate?
Is it possible to deposit Pt directly on Si/SiO2 (PECVD) substrate?
2008-02-16
Steven Yang
Is it possible to deposit Pt directly on Si/SiO2(PECVD) substrate?
2008-02-17
이장근
Is it possible to deposit Pt directly on Si/SiO2(PECVD) substrate?
2008-02-18
Dirk Renckens - TNW
Is it possible to deposit Pt directly on Si/SiO2(PECVD) substrate?
Dirk Renckens - TNW
2008-02-18
Dear Steven,

Personally I have sputtered Pd (which is chemically similar to Pt)
directly on virgin prima Si (with native oxide). The deposited coat
(which was ~20nm in my case) was stable against common organic and
inorganic solvents (ethanol, acetone, water, toluene). I do not know if
it will be stable in piranha, but it is possible (Pt is normally
dissolved in aqua regia). When my Pd layer was exposed to air plasma
(i.e. a mild oxygen plasma), the Pd was initially stable (also in
solvents), but would start to flake when exposed to a reducing agent. I
hope this information helps.

Kind regards,

Dirk Renckens
PhD student - TU Delft

-----Original Message-----
From: Steven Yang [mailto:[email protected]]
Sent: 16 February 2008 10:47
To: mems-talk
Subject: [mems-talk] Is it possible to deposit Pt directly on
Si/SiO2(PECVD) substrate?

Hi, all

Not sure the Pt (sputtering) will stick firmly on the substrate or
not? as normally Ti/Pt is used for the electrode deposit. But I am
going to try Pt directly on Si substrate with PECVD SiO2 (1 or 2 um)
due to machine limitation.


and if possible, will the Pt electrode firm enought to go through some
processes like Piranha, O2 plasma?

Thank you very much!

Steven

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Addison Engineering
Process Variations in Microsystems Manufacturing