su8 cracking
oygm
2008-02-18
Hi, everybody
I tried to coat a 20um su8 mask on glass. Su8-50 is used in this process. After
developing, cracks are observed everywhere on su8. These cracks are run through
the entire su8 layer. It is really wired since I used the same protocol and get
succeed last year.

Here is the procedure I’ve followed:
Plasma cleaning―bakes 20mins @ 200c
Spin coating
Soft bake 3mins @65c, 15mins @95c, cool down to RT in 45mins
Expose 250mj/cm2
Post expose bake 1mins @65c, 4mins @95c, cool down to RT in 45mins
Develop

Also I noticed that the su8 which I used was expired last July. Is the
expiration the explanation for cracking? Or the incorrect exposure dose? Or
something else?

Thanks

--sonic
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Tanner EDA by Mentor Graphics
University Wafer