A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: fialed in borofloat-si bonding?
fialed in borofloat-si bonding?
2008-03-06
ShengYi Hsiao
2008-03-06
Tony Rogers
2008-03-06
Loren St. Clair
2008-03-06
Ruiz, Marcos Daniel (SENCOE)
failed in borofloat-si bonding?
2008-03-07
Brad Johnson
2008-03-10
Brubaker Chad
2008-03-11
Shay Kaplan
fialed in borofloat-si bonding?
ShengYi Hsiao
2008-03-06
Hi everybody.

Does anyone have experience in bonding borofloat glass to silicon wafer?

I am using recipe of 1000V and 400degree celcuse in vaccume environment,

however, after applying  that bonding condition for an hour, the glass and
the

wafer still not being bonded. Only same weak connection randomly happened,

which results the  interfering pattern. The wafers can easily be separated.

Does anyone know the bonding condition for borofloat glass and Si?



the FAIL experiment records are :

voltage : 1000V

temperature:  400C

pressure:  9mtorr

bonding: 1 hr

bonding current: 0.02mA (form starting to the end) ....WHY?

Charge: 0~6e-2 (form starting to the end)


Any help would be greatly appreciated.

Greetings,

IAN Hsiao.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.