Brubaker Chad
Edge Bead Removal
basar bolukbas
2008-03-11
Dear bibbotson.

You can remove your edge beats with a q-tip which dipped into acetone.
But be careful when you clean your samples edge with this q-tip in order to keep
your patterns.

As far as i know, edge beats are very important to reach min. feature size that
you desire during expose.
So you have to remove these beats.

Bye...

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing