A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: PMMA thickness for nanometer size features
PMMA thickness for nanometer size features
2008-03-11
[email protected]
PMMA thickness for nanometer size features
[email protected]
2008-03-11
Hi all,

I'm trying to pattern Bragg gratings through e-beam lithography on a =
SiO2 layer deposited by cvd on silicon. I am using 950PMMA resist from =
Microchem. The minimum feature of the grating is 115nm, the pattern =
needs to be written by ebeam, developed and etched afterwards. I would =
be grateful if you could give me any suggestions for the PMMA thickness. =
As a rule of thumb I knew that thinner PMMA (let's say 100nm) is good =
for higher resolution features, although this could be a problem for the =
subsequent etching step (as the PMMA might be burned away completely =
during the process). What do you think?

Thank you,

R.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
The Branford Group
Harrick Plasma, Inc.