hello all,

i want to wire bond to chromium pads (ebeam
evaporated, 200 nm thick,1 mm x 1mm). The chromium was
exposed to BOE during the fabrication process. I would
like to know the wire material, process conditions and
equipment details.

Any help is appreciated.