Hakemi, Ghazal
2008-03-17
Dear All,

does copper etch anisotropically in FeCl3?
I am trying to achieve relatively straight walls.
Many thanks,

Miss Ghazal Hakemi
PhD Student=20
Microsystems and Nanotechnology Centre (Building 70)
Cranfield University