Hi,

I dissolve my FeCl3 powder into DI water and used the solution =
repeatedly to etch copper with minimum undercut. Adding some HCl to the =
solution helps to reduce some kind of colloid formation. FYI.

Best regards, Tien Khee

________________________________

From: Hakemi, Ghazal [mailto:[email protected]]
Sent: Mon 3/17/2008 10:21 PM
To: [email protected]
Subject: [mems-talk] Cu etch in FeCl3

Dear All,

does copper etch anisotropically in FeCl3?
I am trying to achieve relatively straight walls.
Many thanks,

Miss Ghazal Hakemi
PhD Student=3D20
Microsystems and Nanotechnology Centre (Building 70)
Cranfield University
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Mentor Graphics Corporation
MEMS Technology Review