Steven Yang
2008-03-18
My microfluidic pattern is made of SU-8 on the Si substrate. I tried
to seal the pattern with a piece of PDMS. The PDMS is Oxygen plasma
treated at 20W for 20s to achieve a hydrophlic surface toward the
pattern. and SU-8 pattern also oxygen plasma treated under 100W for 1
minute after its hardbake at 150C. After that, two sides was contact
and hot press at 100C for 2 hours in a vaccum oven.

However, the bonding did not succeed. The problem probably comes from
that the PDMS did not show the adhesive property to SU-8 once they
were contacted. Actually, the PDMS is always show a "stick on" effect
when it is contacted to other materials, such as glass dish, or Si
substrate, even after the oxygen plasma treatment. But when it contact
to my SU-8 pattern surface, the effect did not show up. I read a lot
of work doing SU-8 and PDMS bonding with Oxygen treatment, but why does my
work turns out that the PDMS seems does not have the possibility to be
bonded on it?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review
The Branford Group