A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: removing sticky adhesive
removing sticky adhesive
2008-03-18
Vikrant A. Chaudhari :)
2008-03-18
Jesse D Fowler
2008-03-18
Bill Moffat
2008-03-18
Bill Moffat
2008-03-19
Olgierd Cybulski
2008-03-20
Kagan Topalli
2008-04-03
Bill Moffat
2008-03-21
Brad Cantos
2008-03-20
Alderete, Michael
2008-03-21
Michael Larsson
removing sticky adhesive
Bill Moffat
2008-03-18
Try Oxygen plasma.  Bill Moffat

________________________________

From: [email protected] on behalf of Jesse D Fowler
Sent: Tue 3/18/2008 8:20 AM
To: [email protected]; General MEMS discussion
Subject: Re: [mems-talk] removing sticky adhesive

I would try acetone/alcohol/water.

If that doesn't work, piranha.

"Vikrant A. Chaudhari :)"  writes:

hello,

is there a way to remove sticky adhesive, which is left over after a
cellotape is removed. we are using cello tape for masking while etching
SiN, and when cellotape is peeled of the sticky glue is left over. Is
there a better way to remove it with out scrubbing?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMS Technology Review
MEMStaff Inc.