MEMSnet Home: MEMS-Talk: removing sticky adhesive
removing sticky adhesive
2008-03-18
Vikrant A. Chaudhari :)
2008-03-18
Jesse D Fowler
2008-03-18
Bill Moffat
2008-03-18
Bill Moffat
2008-03-19
Olgierd Cybulski
2008-03-20
Kagan Topalli
2008-04-03
Bill Moffat
2008-03-21
Brad Cantos
2008-03-20
Alderete, Michael
2008-03-21
Michael Larsson
removing sticky adhesive
Kagan Topalli
2008-03-20
O2 plasma removes the sticky glues of cellotapes.
Regards,

Kagan TOPALLI, Ph. D.
Senior Research Engineer
MEMS-VLSI and EMT Group
Middle East Technical University
Dept. of Electrical & Electronics Eng.
TR-06531 Ankara Turkey
Phone: +90 312 210 44 09 or +90 312 210 23 40
Fax: +90 312 210 23 04
http://www.mems.eee.metu.edu.tr/~topalli/
--



Olgierd Cybulski wrote:
>>  is there a way to remove sticky adhesive, which is left over after a
>>  cellotape is removed. we are using cello tape for masking while etching
>>  SiN, and when cellotape is peeled of the sticky glue is left over. Is there
>>  a better way to remove it with out scrubbing?
>>
>
> It depends on the type of glue.  Try IPA, extraction naphtha or benzine.
> Sometimes acetone is enough.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing