Hey Eric,

Thanks for your information. I also had a lot success when humidity is
low. However, it is just annoying to be influenced by this. I am wondering
using some adhesion promoter like AP300 would minimize the influence of
humidity and also give me better adhesion. Hope we could have more
discussions here. Thanks!

Peng

Dept. of Mech. Eng.
Univ. Rhode Island

> Peng
>
> I just had a bad experience with SU8 and humidity.  Ours was up to 55%.  I
> tried spincoating Si wafers with SU8.  It looked good, but shortly after,
> I found it all beaded up on the wafer.  After we fixed the humidity, it
> worked fine.  It should normally be around 10%.
>
> Eric
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
University Wafer
Process Variations in Microsystems Manufacturing