A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: removing sticky adhesive
removing sticky adhesive
2008-03-20
Alderete, Michael
2008-03-18
Vikrant A. Chaudhari :)
2008-03-18
Jesse D Fowler
2008-03-18
Bill Moffat
2008-03-18
Bill Moffat
2008-03-19
Olgierd Cybulski
2008-03-20
Kagan Topalli
2008-04-03
Bill Moffat
2008-03-21
Brad Cantos
2008-03-21
Michael Larsson
removing sticky adhesive
Bill Moffat
2008-04-03
Oxygen plasma is 100% successful in removing sticky tape residue.
Contact me for further details. www.yieldengineering.com ,
[email protected] 925 373 8353.  BillMoffat

________________________________

From: [email protected] on behalf of Olgierd Cybulski
Sent: Wed 3/19/2008 10:57 AM
To: [email protected]; General MEMS discussion
Subject: Re: [mems-talk] removing sticky adhesive

>  is there a way to remove sticky adhesive, which is left over after a
>  cellotape is removed. we are using cello tape for masking while =
etching
>  SiN, and when cellotape is peeled of the sticky glue is left over. Is =
there
>  a better way to remove it with out scrubbing?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
University Wafer