A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Pyrex isotropic etching
Pyrex isotropic etching
2008-04-04
Yoshi Sakata
2008-04-04
Edward Sebesta
2008-04-05
Yoshi.Sakata_Gmail
2008-04-07
Edward Sebesta
2008-04-09
Joseph Grogan
Pyrex isotropic etching
Edward Sebesta
2008-04-04
Wet etch is isotropic when the substrate to be etched is largely or
completely isotropic in nature, such as glass. Some type of flouride
solution should do well. Depending on the type of resist you might want
to use a buffered oxide etch solution which comes either 13:2 or 6:1
from vendors and is known as "BOE".

Ed

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Yoshi Sakata
Sent: Thursday, April 03, 2008 10:28 PM
To: [email protected]
Subject: [mems-talk] Pyrex isotropic etching

Hi,

I'm looking for the isotropic etching method to cut grooves on a pyrex
wafer. The groove will have about 50um depth. I expect that the bottom
and side surface of the groove is smooth. Because I will put the Au
electrodes on those surface. Does someone have a good idea?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
University Wafer
Addison Engineering