Hi Robert,

I recently set-up at electrochemical drilling station in our facilities for
Pyrex glass.  Not sure of your hole requirements (roughness, wall profile,
...), but it seemed to work well if you are interested in just an access thru
the wafer.  10um might be a bit much, but 30-150um might be possible.

Thanks,

Carlos Gonzalez, Ph.D.
Abbott Laboratories
Depart. 46s, Build. AP52 South
200 Abbott Park Road
Abbott Park, IL 60064-3537
(847) 935-5423
(847)937-5500 Fax
[email protected]





[email protected] on 08/17/98 11:10:07 AM
Please respond to [email protected] @ INTERNET
To: [email protected] @ INTERNET
cc:
Subject: Holes in Pyrex

Hi folks.

I looking to drill an array of 10um
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
The Branford Group
Nano-Master, Inc.