PMMA etch resistance
Satish Yeldandi
2008-04-08
Hi all

I am trying to etch SiO2 using PMMA as mask. I am using ICP RIE system for
plasma etching. My oxide layer is 250nm thick and the substrate is Si. PMMA
is 180nm thick. PMMA is not holding as a mask. I am not able to etch SiO2
with this thick PMMA. Can anyone suggest me how to etch SiO2 with this thick
PMMA as mask.

Thanks
Satish
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
Harrick Plasma, Inc.
MEMStaff Inc.