A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Hf resistant Adhesion layer for Au on Si
Hf resistant Adhesion layer for Au on Si
2008-04-03
Heiko Prüßner
2008-04-03
Morrison, Richard H., Jr.
2008-04-03
Ruiz, Marcos Daniel (SENCOE)
2008-04-03
Brent Garber
2008-04-04
Michael Larsson
2008-04-09
Heiko Prüßner
2008-04-09
Shay Kaplan
2008-04-09
Jesse D Fowler
Hf resistant Adhesion layer for Au on Si
Jesse D Fowler
2008-04-09
Ti is vulnerable to HF. So, you may get some (or all) peeling if you use Ti.

Jesse Fowler


"Shay Kaplan"  writes:

Try to use Ti as adhesion layer.

Shay
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Nano-Master, Inc.
The Branford Group