MEMSnet Home: MEMS-Talk: PMMA etch resistance
PMMA etch resistance
2008-04-08
Satish Yeldandi
2008-04-09
Kvel Bergtatt
2008-04-10
Oakes Garrett
2008-04-09
S.M. SAYDUR RAHMAN
2008-04-10
Satish Yeldandi
PMMA etch resistance
Satish Yeldandi
2008-04-10
Hi!

I did not try wet etch. I am concerned about the anisotropy. I am
using PMMA A4 950ml. Its around 180nm thick. I dont know whether a
thicker PMMA will resolve my patterns. My pattern is photonic crystal
structure with 217 nm circles.

Thanks all
satish

On 4/10/08, Oakes Garrett <[email protected]> wrote:
> Have you tried a buffered oxide etch (BOE)?
>
> http://en.wikipedia.org/wiki/Buffered_Oxide_Etch
>
> Best Regards,
> Garrett Oakes
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
MEMStaff Inc.
Harrick Plasma, Inc.