MEMSnet Home: MEMS-Talk: Best plasma chemistry for SiO2/Si selectivity
Best plasma chemistry for SiO2/Si selectivity
2008-04-10
Satish Yeldandi
2008-04-10
Rashmi Rao
2008-04-10
Satish Yeldandi
2008-04-10
Ad Hall
Best plasma chemistry for SiO2/Si selectivity
Satish Yeldandi
2008-04-10
Hi all

I am wondering if someone can suggest me a good plasma chemistry to
get a very good selectivity between SiO2 and Si

I am using Trion's minilock phanthom III series ICP RIE etch system. I
have access to Ar, N2, O2, BCl3, Cl2, CF4 gases.

CF4 is etching both Si and SiO2, even Cl2/BCl3 combination is etching both.

Thanks a lot
Satish
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
Nano-Master, Inc.
MEMS Technology Review