MEMSnet Home: MEMS-Talk: Stress reduction in a multilayers membrane
Stress reduction in a multilayers membrane
2008-04-11
Guillaume Bougrine
Stress reduction in a multilayers membrane
Guillaume Bougrine
2008-04-11
Hello,

I am currently working on a pressure sensor whose membrane is made of SiC, W and
SiO2. After anodic bonding, it came out that the membrane is really stressed
since we do not need a microscope to see the deformation.
Then, I would like to know if someone have any advice or would know papers or
process to get rid of this problem.

Thank you in advance.

BOUGRINE Guillaume
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Nano-Master, Inc.
Addison Engineering