2008-04-17
Yes we do however we also do spin coating of glass and sol-gel both are
much less costlier and faster.
good luck
walter
www.elume.com
----- Original Message -----
From: "Rafael Garcma Valverde" 
To: "General MEMS discussion" 
Sent: Thursday, April 17, 2008 6:31 AM
Subject: [mems-talk] Passivation of ITO with SiO2

Hi everybody,

I know that once ITO is sputtered over glass substrate, some companies
offer it with a thin layer of SiO2 for passivation.

Does anyone know if this layer is also sputtered?

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing