A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Teflon Patterning
Teflon Patterning
2008-04-21
Teimour Maleki
2008-04-21
SEBESTA Edward
Solvent effects on Teflon AF
2008-05-09
Teimour Maleki
2008-05-12
Brubaker Chad
2008-04-21
Bill Moffat
2008-04-21
Michael Larsson
Teflon Patterning
Michael Larsson
2008-04-21
Hi Teimour,

Do what they do to get PTFE to stick to the surface of frying pans -
mechanical interlocking. Roughen-up your Si surface using RIE (you
could try an isotropic recipe, through a mask) prior to PTFE
deposition and this should help.

Regards,

Michael


>
> ---------- Forwarded message ----------
> From: "Teimour Maleki" 
> To: "'General MEMS discussion'"  Date: Sun, 20 Apr 2008 23:34:46 -0400
> Subject: [mems-talk] Teflon Paterning
> Dear all,
>  I am trying to pattern a thin film of Teflon on silicon substrate. I tried
> argon plasma activation, it seems fine, but I have problem with adhesion of
> Teflon to silicon. When I do post processing, it will pill of. Any comments
> on this will be appreciated very much.
> Thanks,
> -Teimour
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
MEMStaff Inc.
Nano-Master, Inc.