A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: SiO2 growth on bare silicon
SiO2 growth on bare silicon
2008-04-19
Jose Guevarra
2008-04-19
Peng Li
2008-04-23
Albert Henning
2008-04-19
Ravi Shankar
2008-04-19
Vossough
2008-04-21
jian zi
SiO2 growth on bare silicon
Albert Henning
2008-04-23
The work published over time by Grove and his colleagues had a 'fitting'
factor, which appeared in the model as an initial oxide thickness, which
they could never explain.

Subsequently, literally a thousand papers were published on oxidation of
silicon.

As a way to sift through this massive pile, I suggest you look for the
articles by Hisham Massoud, who is a professor of EE at Duke, who at one
point had done what was acknowledged to have been the best work on
oxidation of very thin oxide layers.

Sincerely,

Albert K. Henning, PhD
Director of MEMS Technology
NanoInk, Inc.
215 E. Hacienda Avenue
Campbell, CA  95008
408-379-9069  ext 101
[email protected]

-----Original Message-----
From: Jose Guevarra [mailto:[email protected]]
Sent: Friday, April 18, 2008 10:33 PM
To: General MEMS discussion
Subject: [mems-talk] SiO2 growth on bare silicon

Hi,

   I've found that the grove-deal model of oxidation doesn't work well
for growing oxide on bare silicon waters.  What model should I use to
try to find the time to grow say a 200 angstrom layer of oxide (dry
and/or wet)?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Addison Engineering
Tanner EDA by Mentor Graphics