Hi all,

 Currently, I am etching PECVD oxide using standard RIE and Cr is the
masking layer. However, I found that I cannot remove the Cr mask using
Cr etch after going through the RIE process. I am wondering if there
is anything happened on the Cr surface. I'd like to see if you could
give me some suggestions on how to remove the top Cr layer. Thanks

HY
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Addison Engineering
The Branford Group