MEMSnet Home: MEMS-Talk: Gold evaporation coating on silicon.
Gold evaporation coating on silicon.
2008-05-01
Moshe
2008-05-01
Andrea Mazzolari
2008-05-01
Shay Kaplan
2008-05-01
Roger Shile
2008-05-01
Roger Shile
2008-05-01
Kevin Paul Nichols
Gold evaporation coating on silicon.
Roger Shile
2008-05-01
Sorry for the misplaced sarcasm.  I hadn't noticed the word gold in the
subject line.  In this case an adhesion layer of Ti or Cr would be
appropriate.

Roger Shile

-----Original Message-----

That depends.  If you're going to evaporate water the surface should be
hydrophilic.  In this case oxidizing should do the trick.

Roger Shile

-----Original Message-----
Hello

I want to coat silicon with evaporation coating, and
to assurance that the adhesion between the two
materials  will be optimal.
What will be  the optimal treatment to achieve
adhesion ?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing