Hi  Matthew,

Yes, It is so, the strained Silicon has less Si-Si bond energy,
so far as the bond dissociation is concerned. as compared to Single crystal
silicon. Al-though the Reaction  rate (Chemical Reaction) of the Si-F
species remains the same as in the case of Single crystal Silicon, but their
is a difference in the disorption rate of Si-F species from the top surface
of the feature to be etched. therefore, strained silicon can be etched
faster than Single crystal Silicon.

the deference in the desorption rate of Si-F byproducts can lead to the
non-uniformity in etching. this can be minimized by applying extra energy to
the ions during etching cycle of a typical BOSCH process, so that sputtering
coefficient got increased and hence minimize the non-uniformity..

In a typical BOSCH process this can be achieved by simply increasing the
platen power during the etch cycle along with Etch cycle time simultaneously.

Good Luck!

Manish Hooda
SCL India.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering