PR striping after ICP RIE
2008-05-20
Manish Kumar
PR striping after ICP RIE
Manish Kumar
2008-05-20
Satish,

    this happen due to PR reticulation during plasma etching. in that case
normally plasma ashing and chemicals that you have used will not work. In
this case you can use Piranha Solution (H2SO4+H2O2) heated at 110 degree
celcius for about 30 minutes, you can get rid from this problem, but you
can use piranha only if you are not having metal on your sample.

If you have metal than you can use EKC Polymer remover heated at 65 degree
celcius for 15 minutes.

I hope by using this you can be out of trouble.

Good Luck!

Manish Hooda
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics